Abstract

In this paper, the deformation behaviour of Zr65 Cu17.5Ni10Al7.5 metallic glasses with different amounts of free volume was investigated with nano- and micro-indentation. It was found that the plastic flow of the metallic glasses is closely related to the amount of free volume. The metallic glasses with more free volume exhibit more conspicuous serrations with a larger pop-in size during nanoindentation and more pronounced shear bands during micro-indentation. The effect of free volume on the deformation behaviour of the Zr-based metallic glasses is discussed in terms of free volume theory.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.