Abstract

The effect of directional recrystallization on the LCF characteristics of PM nickel-based superalloy APK-6: Godfrey, A. W. and Martin, J. W. Proc. Conf. Superalloys 1992, Champion, Pennsylvania, USA, 20–24 Sept. 1992 (The Minerals, Metals & Materials Society, 420 Commonwealth Dr, Warrendale, PA 15086, USA) 1992 pp 757–764

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.