Abstract
Background : The latest development of dental material restoration is a bulk fill sculptable composite resin. This material can be applied to a 4 mm cavity at once irradiation. The success of polymerization can be affected by improper irradiation. Both the physical and mechanical properties of the material also can be decreased by improper irradiation. This study aimed to determine the effect of different light-cured unit intensities on the depth of polymerization of bulk fills sculptable composite resin restorations.Method : This research method was an experimental analytic type of post-test only control group design laboratory, consisting of 24 bulk fill sculptable composite resin with a diameter of 4mm x 6mm thickness divided into 6 groups:A1(3M ESPE-low intensity),A2(3M ESPE-high intensity),A3(3M ESPE-soft start intensity),B1(Ivoclar vivacity-low intensity),B2(Ivoclar vivadent-high intensity) and B3(Ivoclar vivadent-soft start intensity). Result : The results showed a significant effect of the low, high, and soft start intensity light-cured units in the bulk fill sculptable composite resin groups by Kruskal-Wallis test 0.00 (p <0.05).Conclusion : The best polymerization depth of bulk fill sculptable composite resin was 3M ESPE and it was affected by the high and low-intensity light-cured units
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Similar Papers
More From: Jurnal Medali
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.