Abstract

The aim of the article is to find the optimal fluxing agent for porcelain body regarding to the possibility of the lowest firing temperature. Sintering behaviour of dry pressed test samples made from the mixture of kaolin and three different types of industrially milled feldspar rocks, bone ash and quartz sand with similar granulometry as dependence of water absorption on the firing temperature was investigated. The most intensive fluxing agent for the sintering is bone ash—the mixture containing bone ash (20wt.%) showed sintering temperature 1200 °C. That is about 50 °C lower compared with the most intensive feldspar based fluxing agent—potassium feldspar rock containing 75% of pure microcline.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.