Abstract

The susceptibility to stress corrosion cracking of a CF3 cast austenitic stainless steel, heat treated to generate a range of delta-ferrite contents, and weld metal that contained either 0 or 6% delta-ferrite has been assessed in a buffered, sulphate environment at 250°C using slow strain rate and constant displacement tests under open circuit conditions and at various applied electrode potentials. The susceptibility to cracking of the CF3 material decreased with increasing delta-ferrite content in the range 2–7% and the 0% delta-ferrite weldment was more susceptible to cracking than the 6% weldment. Sensitization increased the susceptibility of the 0% deltaferrite weldment but had little effect on the 6% weldment. Bolt-loaded WOL data for the weldments indicated that the plateau crack growth rates were higher and the K Iscc values lower for the 0% than the 6% delta-ferrite material. Plateau crack growth rates were ~ 10 −7 mm/s for the 6% delta ferrite weldment and ~ 10 −5 mm/s for the 0% delta ferrite weldment. For the test conditions investigated, the CF3 steel was less susceptible to stress corrosion cracking than either of the weldments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.