The rolling process of Bi-2223 tape conductors was optimized through the regressive analysis of experimental data. This procedure ensures the effective densification of the powder precursor in the core and homogeneous distribution of powder density in conductor cross section, thus shortening the rolling process. The Jc values were realized for the monofilament and 19-filament conductors processed by "powder in tube" method with one step intermediate rolling such as 3.1/spl times/10/sup 4/ A/cm/sup 2/ (77 K, OT) and 2.6/spl times/10/sup 4/ A/cm/sup 2/ (77 K, OT) respectively. Characteristics of single pancake coils are presented fabricated from 19-filament conductor: no Jc degradation was observed after 10 steps of thermocycling in the range between 77 and 293 K.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.