The influence of creep deformation of a β sialon with Sm-melilite solution (denoted as M′) as intergranular phase on Vickers hardness, indentation fracture toughness and Weibull modulus was investigated in this article. For samples crept at different temperatures and stresses, Vickers hardness and fracture toughness fell in the range of 14.1–15.5 GPa and 5.73–7.04 MPa m 1/2, respectively. For virgin sample, the Vickers hardness and toughness were 15.8 GPa and 6.08 MPa m 1/2, respectively. Weibull moduli on Vickers hardness were 36 and 39 for the samples crept at 1300 °C (sample 5, see Table 1) and 1350 °C (sample 9, see Table 1), respectively, compared to 23 for the virgin sample. Weibull moduli on fracture toughness were 18 and 21 for sample 5 and sample 9, respectively, compared to 19 for the virgin sample. The discrepancy of Vickers hardness, fracture toughness and Weibull modulus between the virgin and crept samples was due to the more compact microstructure, the decrease in the amount and devitrification of intergranular phase and cavities during creep. Aging effect study shows that Vickers hardness values on the ends of crept specimens are lower than those within the deformation zones.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.