Abstract

Keywords: Boron Carbide; Silisium Carbide; Composite; Powder Metallurgy. Abstract : In this study, effect of boron carbide (B4C), aluminium oxide (Al2O3) and silisium carbide (SiC) addition on microstructure and mechanical properties of diamond cutting segments was investigated. The effects of reinforcement particle additions on characteristic of CuSn matrix composites have been investigated. For this purpose, Al2O3, SiC and B4C addition quantity was added as 2 wt.%. Samples of segments were processed by cold pressing at 550 MPa, followed by sintering at 850°C/30min. Micro-structural aspects were observed by optical microscope. Density, hardness and wear tests were also performed. Wear behaviour and hardness values of segments changed depending on aluminium oxide, silisium carbide and boron carbide addition. The alloy CuSn– 2 wt.%. B4C presented the best results, available for use in cutting tools.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.