Abstract

The basis for the evaluation of polyethylene materials for pressure pipe applications is hydrostatic stress rupture testing for the prediction of long-term hoop strength. However, it is crucially important that the fracture properties of the materials are understood and indeed may result in limitations of their use. Slow crack growth has been recognized in pipelines to result from flaws, notches created during installation, rock impingement and bending loads. This paper outlines the development of the ‘notched pipe test’ for the assessment of the resistance to slow crack growth of polyethylene pipe, carried out by an Ad Hoc Group of ISO/TC138/SC4 (Plastics Pipes - Gas Applications).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.