Abstract

This article discussed the development process and anion release mechanism of anion printing poplin. Through ultra-fine processing and special modification, 6-ring stone and a variety of functional materials were used to process anion additives. The particle size of anion additives is 50-900 nm. Mix the additive and other additives, then modulation into sizing agent. Through experiments and instruments test, the poplin which obtained by an ordinary printing process, is proved has higher wear behavior. At the same time, the poplin can stable and lasting release anion reached 3000/cm3, reach people's health requirements

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.