Abstract

After several repetitions of GaN epitaxial growth, the quality of the AlN template grown by metal–organic chemical vapor deposition deteriorated seriously, even when grown under the same procedure. However, the quality of the AlN template recovered a little the second time. It is found that this deterioration was enhanced if we increase the growth temperature. And this deterioration can be effectively weakened by omitting the baking procedure to cover the reactor chamber with AlN. The full width at half maximum of the X-ray rocking curve for AlN(102) significantly decreased from 1843 to 402 arcsec. This suggests that this deterioration of AlN quality is caused by residual gallium in the reactor chamber.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.