Plate-type phosphor is a promising substitute in overcoming the issues related to the powder phosphor paste mixed with resin. In this research, Ca-α-SiAlON:Eu 2+ plate phosphor (CaxSi 12-(m+n) Al m+n O n N 16-n :Eu y ) was investigated for the varied compositions (m,n) of the host crystal with the fixed Eu content (y). Densification was promoted for the compositions with increasing ‘m’ values for the m=2n relationship. Dictated by the Eu concentration inside the phosphor crystal, photoluminescence intensity was stronger in α2 specimen (m = 3.0, n = 1.5) containing the second phases when compared to α1 specimen (m = 1.5, n = 0.75) comprising a single-phase α-SiAlON. The concentration of Eu in the non-emitting amorphous interfacial glass phase was 2~4 times of the designed Eu concentration inside the α-SiAlON crystal.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.