Abstract
In this paper, a novel approach, proposed for predicting residual stresses induced on materials treated with high pressure water jets, i.e. water jet peening, is presented. This approach considers the impact pressure distribution due to high velocity droplets impinging on the material surface instead of stationary pressure distribution considered in Trans ASME J Eng Mat Technol 121 (1999) 336 for prediction of residual stresses on water jet peened surfaces. It makes use of Reichardt’s theory for predicting the velocity distribution of droplets and liquid impact theory for predicting the impact pressure and duration of impact of high velocity droplets. For predicting residual stresses on the surface and sub surface of material subjected to water jet peening, finite element modelling approach was adopted by considering the transient, dynamic nature of droplets for analysis. The effectiveness of the proposed approach was demonstrated by comparing the predicted residual stresses with those predicted employing the approach proposed in Trans ASME J Eng Mat Technol 121 (1999) 336. Finally, the practical relevance of the proposed approach was shown by comparing the predicted results with the experimental results obtained by water peening of 6063-T6 aluminium alloy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.