In the present work, CAS (CaO–Al2O3–SiO2)-based glass–ceramics were prepared by using Al2O3 (Seydisehir, Turkey) and pumice (Nevsehir, Turkey) as natural raw materials and marble dust (Sakarya, Turkey) as a waste source. CAS-coded composition (57.5 mass% SiO2, 27.5 mass% CaO, 15 mass% Al2O3) was selected in stoichiometric anorthite region according to the CAS ternary diagram. According to the DTA results at different heating rates, the crystallization activation energy of the glass that was prepared from the CAS-coded composition was calculated to be 373 ± 5 kJ mol−1 and the viscous flow activation energy to be 430 ± 8 kJ mol−1.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.