Abstract

The manufacture method based on the silicon etching process is one of the most important methods to fabricate micro mechanical structure, e.g. micro-engine. In the processing, the high aspect ratio silicon etch process (HARSE process) is very important to improve the efficiency of structure. At the same time, the surface morphology should be controlled exactly to keep the performance of structure. In this paper, the feasibilities of controlling the surface morphology and Si etch rates were experimentally investigated. In the experiments, the width of structure changes from 15um to 1500um and the depth changes from 50um to 500um. The parameters of surface morphology including sidewall angle, surface roughness, and so on were measured and compared. The influence mechanisms of etching parameters were analyzed. The etching process were completed in a surface technology system (STS) multiplex advanced silicon etcher inductively coupled plasma (ICP) system with SF6/O2 plasma as etching plasma and C4F8 as passivation plasma. In the experiments, the etching experiments were conducted in a low pressure (5–50mTorr), high density, inductively coupled plasma etching reactor (ICP) with a planar coil. The Si etches rates and sidewall angle were investigated as a function of chamber pressure, cathode RF-power, and gas flow. The results indicated that the increasing of total etching time results in an acceleration in etch rate as well as the decrease in sidewall angle (the top width of trench is narrow than the bottom width). Meanwhile, the total passivation time has an opposite effect in the influence of etch rate and sidewall angle. All the experiments indicate that the quick shift between etch and passivation period leads to a smoother surface. An interesting phenomenon were discovered that the etch rate will not change with the changing of width parameter in most of the high aspect ratio silicon etch recipes when the width-depth ratio is upper than 0.34. An experiential function formula were fitted based on four parameters, including width and depth of the structure, and total etching and passivation time.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.