Abstract

In this study, three polyurethanes (PUs) were synthesized, named PU-31, PU-35 and PU-41, whose tensile strength and modulus increased with the increasing hard segment content. The effect of different loads on wear behavior was investigated systematically. The results showed that the volume loss of PU-31, PU-35 and PU-41 were 1.84, 2.10 and 2.67 mm3 at 5 N load and 68.40, 53.67 and 42.34 mm3 at 120 N, respectively. It found that under low load, PU-31 with low modulus exhibited the best wear resistance. While under high load, PU-41 with high tensile strength was the best. This study revealed that the wear resistance was heavily dependent on the loads, which was crucial for improving the wear resistance of materials according to operation conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.