Abstract
Residual stresses due to surface treatment are measured using the compliance method. The method makes use of the strains measured on the surface while a cut is extended progressively along a plane of interest. The experimental results for a shot peened specimen show good agreement with those obtained by the X-ray method. This experiment demonstrates that the compliance method is accurate and capable of measuring residual stresses which vary rapidly over a depth of less than 50 μm. Good general agreement with results by the X-ray method is also obtained for a laser treated specimen. Some advantages and disadvantages of the present method relative to hole-drilling, layer removal and X-ray methods are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.