Abstract

The fastness of 5% omf dyeings of three indigoid vat dyes on PLA fabric to repeated washing at 40 °C, 50 °C, and 60 °C increased with increasing temperature of their application (60 °C, 80 °C, 98 °C and 110 °C). Fastness to repeated washing at 40 °C and 50 °C was better than at 60 °C. Of the three dyes used, C.I. Vat Blue 35 displayed lowest fastness to repeated washing and also lowest colour strength. Comparison of the fastness results on PLA fabric with those of dyeings of three disperse dyes on PLA fabric as well as dyeings of three other vat dyes on PA supermicrofibre revealed both similarities and differences in terms of colour loss and staining of adjacent materials, which highlighted the likely importance of subjecting vat dyeings on PLA fabric to a clearing process in order to remove surplus dye.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.