Abstract

Zinc is extracted from oxidized ores with solution, and the zincate electrolyte is purified with zinc powder and lime. The zinc is recovered electrolytically as “flake” powder consisting of pinnate crystals. At 12.9 amp/dm2 (120 amp/ft2) about 1.5 kw hr/lb of zinc is required. Many types of oxidized ores have been tested in the laboratory and some pilot‐plant work has been done; the process appears to be feasible.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.