Abstract
A barrier height of 1.13±0.03 eV was measured for Al and Au rectifying contacts to p-type chemical-vapor-deposited diamond thin films using the internal photoemission technique. The results are compared with experimental data reported for Schottky barriers on single-crystal diamond.