Abstract

Measurements of austempering kinetics and mechanical properties are presented as a function of austempering time over the range 1–4320 min for different combinations of austempering temperature (275, 315, 370 and 400 °C) and austenitizing temperature (870, 900 and 950 °C) for a ductile iron of composition 3.5% C, 2.6% Si, 0.48% Cu, 0.96% Ni, 0.27% Mo and 0.25% Mn. The austempering kinetics are used to calculate processing windows for the three austenitizing temperatures. The mechanical properties are analysed to show that the processing windows accurately predict the austempering times over which the mechanical properties satisfy the ASTM standard. The analysis shows the role of austenitizing temperature, austempering temperature and time in optimizing the mechanical properties.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.