Abstract
The innovative method for weld defect classification based on rough set theory is presented in this study. The classification rules have been generated by processing of data base composed of 640 radiographic images referring to certain welding process in aircraft industry. The obtained accuracy of defect identification (from 88% up to 100%, depending on class of defect and choice of classifier) can be evaluated as at least competitive or even better one comparing to results referring to other type of frequently “exploited” classifiers, those mentioned in attached overview section. The identification of weld defects is the final operation which is premised by complicated “chain” of consecutive operations transforming primary radiographs to the form enabling calculation of conditional attributes. That is why brief description of process of transformation of primary radiographs to the forms which are suitable for attributes calculation is included in the paper.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.