Abstract
Lindemann's rule was applied to the α phase of Cu-Zn, Cu-Al, Ag-Mg, Ag-Zn and Ag-Cd alloys, and was found to be valid for these alloy systems. X m > is about 0.2 of the radius of the Wigner-Seitz cell.