Abstract
Degradation of relatively large particle size, 0.5 mm of Type-G PMMA (Rohm and Haas) were conducted with thermogravimetric analysis and evolved gas measurements using quadrupole mass spectrometer under conditions of mass transport limitation. In addition, differential thermal analysis was performed in order to furnish information with regards to exothermic or endothermic reactions associated with the degradation. The tests were conducted in an inert environment of pure N2 and oxygenated environment. The results indicated one step degradation process in pure N2 and the degradation process is endothermic. As the O2 fraction increases the degradation process is transformed to exothermic.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.