Abstract

This paper reports the texture development in Si3N4 by strong magnetic field alignment (SMFA), using slip casting of α-Si3N4 raw powder (SN-E10) and pressureless sintering. The texture of β-Si3N4 in the green and sintered bodies was characterized by X-ray diffraction analysis (XRD) and scanning electron microscopy (SEM). The a, b-axis and c-axis aligned β-Si3N4 has been obtained by the static and rotating magnetic field of 12 T, respectively. The β-seed addition and prolonged sintering both enhance the texture, but the former is more efficient. This work suggests an efficient SMFA strategy of producing highly textured β-Si3N4, particularly the unidirectionally c-axis aligned β-Si3N4 by seeding the α-raw powder using the less-agglomerated β-phase particles.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.