Abstract

Nanocrystalline 4‐mol%‐Sc2O3‐stabilized zirconia (4ScSZ) and 4‐mol%‐Y2O3‐stabilized zirconia (4YSZ) powders were prepared by a mild urea‐based hydrothermal method. The as‐prepared 4ScSZ and 4YSZ powders behaved with different tetragonal–monoclinic (t–m) transitions on calcination at temperatures between 400° and 1400°C. For the as‐calcined 4ScSZ samples, the monoclinic phase fraction varies discontinuously with increasing temperature, i.e., first increases, then decreases, and finally increases again; whereas the monoclinic phase content reduces monotonously for the as‐calcined 4YSZ samples, and only tetragonal phase is present over 1000°C. Such interesting results can be explained satisfactorily by considering the combined influences of crystallite size effect, microstrain, and the stabilization effect of the dopant. The microstrain relaxation is mainly responsible for the unusual phase transition in the 4ScSZ samples, while for the 4YSZ samples, the microstrain effect and crystallite size effect can be masked by the stabilization effect of the Y2O3 dopant due to its stronger stabilization capability.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.