The sorption of Hg(II), Cd(II), and Pb(II) as anionic complexes on the solid phase of polyacrylonitrile fiber filled with the AV-17 anion exchanger from NaCl and KI solutions and their complexation with 4-(2-pyridylazo)resorcinol (PAR) and dithizone were studied. A test method was developed for the individual determination of Hg(II), Cd(II), and Pb(II) from one sample on three support disks. From the same solution, by the successive sorption on two disks from a 0.2 M NaCl solution, mercury was determined with dithizone and cadmium was determined with PAR. After the addition of a KI solution and sorption on the third disk, lead was determined with PAR. Using the added-found method, the procedure was approved in the analysis of natural sodium chloride water. The detection limit was 0.01 mg/L for Hg(II) and 0.02 mg/L for Cd(II) and Pb(II) for a volume of the analyzed sample of 25 mL. The time of the analysis of five or six samples (determination of three elements) is no longer than 50 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.