Abstract
Abstract The article presents the alternative use of termite mound soils (TMSs) as full replacement for clay soils in brick production. TMSs from two localities, Jawaj and Sene, in Ethiopia were investigated for bricks production. The TMSs samples contained high SiO2 and Al2O3. The TMSs bricks were fired at different temperatures from 500 to 1,000°C. The obtained mean compressive strengths (σ), 18 and 14 MPa, were observed for bricks made from TMSs from Jawaj and Sene, respectively, at the optimum firing temperature of 700°C. The σ of TMSs bricks decreased as the firing temperature increased above 700°C, while for conventional clay soil brick, the σ increased with temperature beyond 700°C. The water absorptions and saturation coefficients of fired TMSs bricks decreased with increased firing temperature. The TMSs bricks meet the standard specification of dimension tolerance only along the height. All the TMSs bricks made from the two localities were not efflorescent. TMSs from Jawaj and Sene sites can be used as a raw material to replace the long-used clay soils for bricks production as a construction material for houses construction in rural and urban areas.
Highlights
The article presents the alternative use of termite mound soils (TMSs) as full replacement for clay soils in brick production
TMSs can be considered as suitable raw materials for brick production
TMSs can be used as alternative materials for the production of bricks. – Jawaj termite mound soils (JTMSs) and Sene termite mound soils (STMSs) are classified as A6 according to the AASHTO Classification System
Summary
Abstract: The article presents the alternative use of termite mound soils (TMSs) as full replacement for clay soils in brick production. TMSs from two localities, Jawaj and Sene, in Ethiopia were investigated for bricks production. The TMSs bricks were fired at different temperatures from 500 to 1,000°C. The obtained mean compressive strengths (σ), 18 and 14 MPa, were observed for bricks made from TMSs from Jawaj and Sene, respectively, at the optimum firing temperature of 700°C. The σ of TMSs bricks decreased as the firing temperature increased above 700°C, while for conventional clay soil brick, the σ increased with temperature beyond 700°C. The water absorptions and saturation coefficients of fired TMSs bricks decreased with increased firing temperature. TMSs from Jawaj and Sene sites can be used as a raw material to replace the longused clay soils for bricks production as a construction material for houses construction in rural and urban areas
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.