Abstract

Tensile tests were performed on precracked Cr–Mo martensitic steel (C: 0.38, Si: 0.22, Mn: 0.84, P: 0.024, S: 0.021, Ni: 0.08, Cr: 1.11, Mo: 0.15, Cu: 0.12, Fe: bal. (wt%)) specimens at various strain rates (ranging from 6.5 × 10−8 s−1 to 1.0 × 10−4 s−1) in high-pressure (95 MPa) hydrogen and helium atmospheres. Irrespective of the strain rate, the tensile strength in the helium atmosphere was 1400 MPa. In the hydrogen atmosphere, the tensile strength decreased to less than 600 MPa at a strain rate of 2.0 × 10−5 s−1. However, the tensile strength increased to 900 MPa when the strain rate was decreased to 6.5 × 10−8 s−1. This recovery of the tensile strength was because of the decrease in the local stress in the vicinity of the precrack because of hydrogen.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.