Novel carbon/glass hybrid thermoplastic composite rods consisting of unidirectional PAN-based carbon fiber (T700SC), braids of E-class glass fibers, and thermoplastic epoxy matrix have been developed. Three types of hybrid rods with differing carbon/glass ratios (24K1P, 24K2P, and 24K3P) were fabricated. The cross-sectional morphologies of the hybrid rods were observed using a digital microscope. Volume fractions of carbon fiber, glass fiber, matrix, and void of the hybrid rods were estimated using a specific gravity measurement via ethanol immersion and a thermogravimetric analysis.The tensile properties and fracture behavior of the hybrid rods were investigated. For all hybrid rods, the stress applied to the specimen was nearly linearly proportional to the strain until failure, with a tensile modulus of 65 (24K1P), 87 (24K2P), and 91GPa (24K3P) and tensile strengths of 1.42 (24K1P), 1.80 (24K2P), and 1.84GPa (24K3P). The tensile modulus and strength increased with increasing carbon fiber volume fraction. The Weibull statistical distribution of tensile strength for the hybrid rods was examined. The Weibull modulus of the tensile strengths for the hybrid rods were 23.77 (24K1P), 27.29 (24K2P), and 32.50 (24K3P). The Weibull modulus increased with increasing tensile strength and decreasing void volume fraction of the hybrid rods.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.