Abstract

This paper presents the test results of an experimental study that investigates the durability of a new generation of Glass Fiber Reinforced Polymer (GFRP) bars. A total of 60 GFRP bars were embedded in concrete prisms and exposed to ten environmental conditions for 6 and 12 months. The environments included exposure to ordinary tap water, sea water, and alkaline solution at two temperatures (room and 50°C). The environments also included two typical field conditions of the Kingdom of Saudi Arabia (Gulf area and Riyadh area). The performance of the GFRP bars was evaluated by conducting tensile tests on the bars extracted out of the concrete specimens after exposure to the environmental conditions. After 12 months of exposure, the test results showed that the tap water at 50°C had the maximum effect on the tensile strength of the GFRP bars. The two field conditions did not show any harmful effect on the tensile properties of the bars after 12 months of exposure.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.