Tensile stress–strain properties of Al alloy 6061-T6 (AA6061-T6) and its butt welds produced by the friction stir welding (FSW) process were characterized in two different loading orientations. AA6061-T6 FS welds were made under three sets of welding conditions. Micro-hardness tests were performed to investigate microstructural evolution during the FSW process. Flat tensile specimens were machined normal and parallel to the weld line. Transvers and longitudinal tensile tests were run on the base material (AA6061-T6) and its FS welds in an Instron testing machine. The strength and ductility (or fracture strain) of the FS welds observed in the transverse orientation were substantially less than those in the longitudinal orientation. Constitutive modelling of uniaxial tensile stress–strain behaviour in both orientations was presented using a rate-independent Ludwik equation. In addition, microstructures of the base material and its FS welds were examined with optical and transmission electron microscopy to discuss the decrease in the flow stress level and the increase in the strain hardening rate of the FS welds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.