Abstract
Through experimental study on creep characteristics of conductors with large aluminum-steel section ratio, the creep characteristic curve of conductors with aluminum-steel section ratio between 11.34 and 14.47 are obtained. It is recommended that the conductor should have a temperature-reduction value of 25°C according to the conductor temperature-reduction value analyzed by amount of creep, which can be used for reference during line design and construction.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.