Abstract

In this paper, dynamic compaction is employed to produce Mg–SiC nanocomposite samples using a mechanical drop hammer. Different volume fractions of SiC nano reinforcement and magnesium (Mg) micron-size powder as the matrix are mechanically milled and consolidated at different temperatures. It is found that with the increase of temperature the sintering requirements is satisfied and higher quality samples are fabricated. The density, hardness, compressive strength and the wear resistance of the compacted specimens are characterized in this work. It was found that by increasing the content of nano reinforcement, the relative density of the compacted samples decreases, whereas, the micro-hardness and the strength of the samples enhance. Furthermore, higher densification temperatures lead to density increase and hardness reduction. Additionally, it is found that the wear rate of the nanocomposite is increased remarkably by increasing the SiC nano reinforcement.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.