Abstract
AbstractThe strain distribution in a new generation nickel-based single crystal superalloy has been determined in the temperature range 293 K– 1598 K. Measurements have been performed using diffraction of high energy synchrotron radiation (150 keV,λ= 0.008 nm) to determine the variations with temperature of the γ/γ′ lattice mismatch and of the γ′ volume fraction. The chemical segregation at the dendrite scale and the internal stress induce a large range of values for the lattice mismatch. The measurements of the γ′ volume fraction determined by X-ray diffraction are in agreement with those obtained by atom probe tomography, image analysis or computation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.