Abstract A study was made of the effect of the surface temperature of the rolls of a 6 × 12-inch laboratory mill on the properties of GR-S compounds and means of controlling this temperature. It was found that the properties of the GR-S compound depend on the surface temperature of the mixing rolls. No practical method of controlling the temperature of conventional rolls was found because of the slow rate of heat transfer. Therefore three types of special rolls, including one designed at the National Bureau of Standards, were investigated. The heat transfer characteristics of the NBS rolls permitted automatic control of their temperatures to within 7° F during mixing of natural rubber and several synthetic elastomers, with only one controller being used. A mill with the special NBS rolls has been in operation for about a year, and has resulted in a marked improvement in the control of mixing of rubber compounds. The automatic temperature control has been much more convenient than manual control, and has saved considerable time, since the rolls do not have to be warmed by milling scrap rubber.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.