A complex transmission electron microscopy (TEM) study of reactor vessel internal (RVI) materials from the baffle-former-barrel assembly from NPP Greifswald (VVER 440), Unit 1 decommissioned after 15 service cycles has been undertaken. All parts of the baffle-former-barrel assembly are made from Ti-stabilized austenitic stainless steel 08Ch18N10T. The materials were exposed to different dose of neutron radiation (2.4-11.4 dpa) at temperatures 267-398°C depending on position in the core. Three types of radiation induced defects were identified and quantified, namely: dislocations, cavities (voids) and fine-scaled precipitated particles of Ni-Si rich phases. Black-dot type defects were observed too. Operation conditions are around ≈ 300°C that is why we have observed defect typical for both low and high regions of irradiation temperatures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.