Abstract

The article discusses methods for the preparation of chemically reactive mass LiCoO2 in the form of dispersion for use in chemical current sources. The dispersion technique and the method of deposition of LiCoO2 particles from the obtained dispersion on the electrode material are described. The results of SEM on the penetration of LiCoO2 into the material and the results of mass changes are presented.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.