Abstract
The Sr2ZnSi2O7 ceramics sintered at 1475°C has ɛr=8.5, Qu×f=105,000 GHz (at 12.63 GHz), and τf=−51.5 ppm/°C. The sintering temperature of Sr2ZnSi2O7 has been lowered to 875°C by the addition of 20Li2O–20MgO–20ZnO–20B2O3–20SiO2 (LMZBS) glass. Addition of a small amount of SrTiO3 lowered the value of τf. Tapes were cast using the composition Sr2ZnSi2O7+15 wt% LMZBS. The stacked and sintered tapes exhibited ɛr∼7 and tan δ∼10−3 at 290 K. The chemical compatibility of Ag with the ceramic–glass composites was also investigated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Applied Ceramic Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.