The influence of deposition power and seedlayer on the properties of hard magnet Co 50Pt 50 was studied. Co 50Pt 50(/Co 90Fe 10)/Ru/Co 90Fe 10 trilayer was used as pining/pinned layer in spin valves. The influences of different hard layer, soft layer and free layer on exchange bias, interlayer coupling, and magnetoresistance (MR) ratio were studied. Weak antiferromagnetic interlayer coupling was obtained by adjusting the thickness of hard and soft layers. MR of a spin valve with structure Cr2/CoFe0.5/CoPt4/CoFe0.5/Ru0.8/CoFe2.2/Cu2.05/CoFe2.6/Cu1.1/Ta1 reached 10.68% (unit in nm), which is comparable to those of IrMn-based synthetic spin valves. The increment of the coercivity of the free layer is mainly due to the static magnetic interaction between the hard layer and the free layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.