Co-preparation method has been applied to synthesize nano LaAlO 3 powders. By using La(NO 3) 3 and Al(NO 3) 3 as raw materials and keeping the pH≈9, the co-preparation process could be finished at room temperature. Pure LaAlO 3 nano powders with a size of about 50 nm could be obtained after calcining at 700–800 °C. These nano LaAlO 3 powders could be sintered at 1550 °C for 4 h, a high relative density of about 97% could be reached.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.