Numerous technical, economic and societal factors limit the recycling of waste soda-lime-silica glass back into the primary production process and accordingly alternative applications for this material are sought. This study demonstrates that waste soda-lime-silica container glass is a suitable feedstock material for the production of tobermorite, a calcium silicate cation exchanger. Tobermorites were synthesised at 100 degrees C from stoichiometric mixtures of container glass and lime under alkaline hydrothermal conditions. Increasing concentrations of sodium hydroxide (between 1.0 M and 4.0 M) in the reaction mixture promoted the formation and crystallisation of tobermorite, and also resulted in greater fragmentation of the silicate chains along the b-axis direction. The maximum removal capacities of these tobermorite specimens for Cd2+ (441 mg g(-1)) and Zn2+ (122 mg g(-1)) compared well with those of other waste-derived sorbents. Superior Cd2+- and Zn2+- uptake capacities and kinetics were observed for the least crystalline tobermorite specimen, indicating that stacking defects facilitate the transport and exchange of cations within the lattice.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.