A series of Ba1-xSrxMyTi1-yO3 (M = Zr, Sn, 0⩽x⩽0.4, 0⩽y⩽0.3) solid solutions were synthesized with the soft chemical method below 100 °C. XRD pattern and cell parameters-composition figures of the prepared powder demonstrate that they are completely miscible solid solutions based on BaTiO3. Furthermore, TEM shows that they have a shape of uniform, substantially spherical particles with an average particle size of 70 nm in diameter. The sintered ceramics of the powder doped with Sr2+and Zr4+ or Sn4+ have dielectric constant eight times higher and dielectric loss thirty per cent lower than those of pure BaTiO3 phase at room temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.