Abstract

In this paper we report on the preparation and characterization of porous ceramic substrates in the group of NaZr 2(PO 4) 3, CaZr 4(PO 4) 6, SrZr 4(PO 4) 6 and BaZr 4(PO 4) 6 with low thermal expansion coefficients. The starting powders were obtained by a sol–gel process and attrition milling both before and after calcination. The resulting sintered bodies exhibited high porosity also after further thermal treatments at high temperature. On the other hand their thermal expansion coefficient (CTE) is low over the range 25–1000 °C. In particular the blend between NaZr 2(PO 4) 3 and SrZr 4(PO 4) 6 has a CTE close to zero in the whole temperature range. According to these properties the above mentioned materials seem to be potential candidates as ceramic substrates for catalytic applications in combustion reactions since they maintain a high level of micrometric porosity when operating at temperatures exceeding 1000 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.