Abstract
Design and synthesis of supramolecular hybrids with low dimensionality is currently an attractive research topic. The reaction of Schiff base metal complex with isopolymolybdate leads to the isolation of a new isopolymolybdate based supramolecular hybrid, [Mn(salen)(H2O)2]2[Mo8O26]Na2·2H2O (1) (salen = N,N'-bis(salicylidene)ethylenediamine). The supramolecular hybrid was characterized by single crystal X-ray structure analyses, elemental analyses and X-ray crystallography. Crystal data for 1: triclinic, P-1, a=10.0206(8)Å, b = 11.7416(10)Å, c= 13.1494(13)Å, V = 1382.8(2)Å3, Z= 1, Rgt(F) = 0.0353 and wRref(F2) = 0.1009. Structural analyses reveal that 1 represents the first example of [Mo8O26]4- chains formed POM-Schiff-base hybrid. Hirshfeld surface analysis and fingerprint plots are used for decoding intermolecular interactions in 1. Additionally, magnetic property of 1 indicates that there is an antiferromagnetic coupling between the metal centers in the complex.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have