Pure ZnO and Al-doped ZnO nanomaterial have been successfully fabricated using zinc acetate dihydrate in a basic aqueous solution of KOH through solution precipitation method then treated at 600°C in air. The XRD analysis confirms the Wurtzite hexagonal crystal structure of the product with crystallite size in 32–53 nm range. The morphology of the product has been studied under scanning electron microscopy (SEM). The simultaneous differential scanning calorimetry and thermogravimetric analyses were used to investigate thermal decomposition temperature and different phase transitions up to 800°C. The optical properties and variation in band gap of ZnO by Al doping were investigated by ultraviolet–visible spectroscopy.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.