Abstract

Ultrafine TaC powders were synthesised by spray drying using tantalum oxalate solution. The spray dried powders were spherical shape and less than 30 in size. The powders calcined at 500 and X showed amorphous structures and phase was obtained by calcining at . The particle size and shape remains constant after calcination. The calcined spherical powders were composed of an agglomerate of primary particles under 50 nm in size. The complete formation of TaC could be achieved by heat treatment at for 6 hrs. The observed size of TaC powders by TEM was less than 200 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.