Abstract
The compound super absorbent resin was synthesized by starch, bentonite, acrylic acid and acrylamide, using microwave irradiation. Some key factors affecting the solution absorbency of the polymer such as the amount of bentonite, acrylamide, initiator and cross-linking agent have been discussed. The results showed that the optimal reaction conditions of cross-linking agent, initiator, neutralization degree, bentonite, phosphate starch are 0.045%, 0.32%, 70%, 10%, 3% when the weight ratio of acrylic acid and acrylamide was 2:1, the microwave power was 800W, the radiation time was 15min. Under the conditions, the pure water absorption rate of super absorbent resin was up to 796g/g. when the weight ratio of acrylic acid and acrylamide was 1:1, the absorption rate of 0.9% NaCl was 95g/g.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.