Spherical carbon nanoparticles were synthesized by sol-gel polymerization of resorcinol and formaldehyde in the presence of CTAB(cetyltrimethylammonium bromide) and subsequent carbonization at 900°C. It is found that the amount of CTAB, water and catalyst showed a significant impact on the morphology and size of carbon nanoparticles. According to the BET surface area and capacitance, the nanoparticles were divided into two groups. The carbon nanoparticles with surface area of 725-758 m2/g showed capacitance between 120-140 F/g, while those with surface area of 596-649 m2/g showed capacitance only 60-80 F/g. Difference in the pore size of 1.5 nm to 3.0 nm probably contributed to the difference of capacitance.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.