Micron-sized nonporous silicon carbide (SiC) powder of the spent heating elements of a graphite furnace were used as the common precursor of two different forms of carbide-derived carbon (CDC) synthesized by chlorination at different temperatures: (1) graphitic and (2) amorphous Si-CDCs. Whereas the former material having high electroconductivity was used as an efficient electrode of a microbial fuel cell (MFC), the latter material having high specific surface area was used as an efficient adsorbent for aqueous hexavalent chromium (Cr(VI)). The MFCs generated a significantly high maximum power density of ∼1570 ± 30 mW/m2 and open circuit potential of ∼460 ± 5 mV. The adsorbents exhibited a significantly large adsorption capacity of ∼95 ± 5 mg/g. This study has developed for the first time two types of Si-CDCs having different physicochemical characteristics, from the common SiC precursor via the facile route of different temperature conditions, for bioelectricity generation and environmental remediation a...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call